TY - GEN
T1 - Impact of the Biaxial Stretching on the Breakdown Strength of Polypropylene Films
AU - Zhen, Yijun
AU - Zhou, Bin
AU - Liu, Peiyan
AU - Qiao, Yi
AU - Feng, Yang
AU - Li, Shengtao
N1 - Publisher Copyright:
© 2025 IEEE.
PY - 2025
Y1 - 2025
N2 - Biaxially oriented polypropylene (BOPP) film, as one of the most widely used energy storage materials in capacitor applications, exhibits excellent dielectric properties that are critically influenced by its stretching processes. This study investigates the effects of the biaxial stretching process, including stretching modes and stretching ratios, on the breakdown strength of BOPP films. By analyzing the crystalline characteristics of polypropylene films with different processing parameters, we explore the underlying mechanism between microstructures and breakdown strength of BOPP films. The experimental results demonstrate that under the condition of sequential biaxial stretching, the breakdown strength of BOPP films with a higher stretching ratio is significantly enhanced because of the increased crystallinity and reduced grain size. Specifically, the BOPP film sample prepared with sequential stretching at a stretching ratio of 3.0 × 3.0 exhibits the highest breakdown strength of 696.3 kV mm.
AB - Biaxially oriented polypropylene (BOPP) film, as one of the most widely used energy storage materials in capacitor applications, exhibits excellent dielectric properties that are critically influenced by its stretching processes. This study investigates the effects of the biaxial stretching process, including stretching modes and stretching ratios, on the breakdown strength of BOPP films. By analyzing the crystalline characteristics of polypropylene films with different processing parameters, we explore the underlying mechanism between microstructures and breakdown strength of BOPP films. The experimental results demonstrate that under the condition of sequential biaxial stretching, the breakdown strength of BOPP films with a higher stretching ratio is significantly enhanced because of the increased crystallinity and reduced grain size. Specifically, the BOPP film sample prepared with sequential stretching at a stretching ratio of 3.0 × 3.0 exhibits the highest breakdown strength of 696.3 kV mm.
KW - BOPP films
KW - Breakdown strength
KW - Crystalline characteristics
KW - Stretching process
UR - https://www.scopus.com/pages/publications/105015832524
U2 - 10.1109/ICEMPE66159.2025.11123071
DO - 10.1109/ICEMPE66159.2025.11123071
M3 - 会议稿件
AN - SCOPUS:105015832524
T3 - 2025 IEEE 5th International Conference on Electrical Materials and Power Equipment, ICEMPE 2025
BT - 2025 IEEE 5th International Conference on Electrical Materials and Power Equipment, ICEMPE 2025
PB - Institute of Electrical and Electronics Engineers Inc.
T2 - 5th IEEE International Conference on Electrical Materials and Power Equipment, ICEMPE 2025
Y2 - 3 August 2025 through 6 August 2025
ER -