High-temperature corrosion behavior of S30432 and TP310HCbN coatings in simulated 620°C ultra-supercritical boiler coal ash/gas environment

  • Yugang Liu
  • , Yinhe Liu
  • , Chunhong Mo
  • , Minqiang Zhang
  • , Meng Dong
  • , Shaocheng Pan
  • , Shenming Ran
  • Xi'an Jiaotong University
  • Clean Combustion and Flue Gas Purification Key Laboratory of Sichuan Province
  • Sichuan Dongfang Boiler Group Co., Ltd.

Research output: Contribution to journal › Article › peer-review

6 Scopus citations

Abstract

The high-temperature sulfur corrosion resistance of S30432 and TP310HCbN typically used in the superheater and reheater of a 620°C ultra-supercritical boiler is investigated in this study. Samples coated with coal ash are placed in a device filled with simulated flue gas at 650°C and 700°C, respectively, for 2000 h. The samples are then analyzed through X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy. S30432 is mainly oxidized under 650°C and 0.2% SO2 volume concentration, and the weight reduction is 6.6 mg cm−2. However, under 700°C and 0.3% SO2 volume concentration, severe sulfidation reaction occurs, sharply accelerating high-temperature corrosion. As a result, weight reduction up to 41.8 mg cm−2 occurs. Although sulfidation reaction also occurs in TP310HCbN, there is no serious corrosion; the corrosion rate reduces in the later stages of the experiment, and a weight increase of 2.4 mg cm−2 is observed. After 11 520 h of the actual operation of the 1000 MW 620°C boiler, there is no obvious high-temperature corrosion in the high-temperature areas without coke-block adhesion. These results indicate that S30432 and TP310HCbN satisfy the requirements of 620°C ultra-supercritical boilers burning high-sulfur coal.

Original languageEnglish
Pages (from-to)1222-1235
Number of pages14
JournalMaterials and Corrosion
Volume73
Issue number8
DOIs
StatePublished - Aug 2022

Keywords

  • 620°C boiler
  • S30432
  • TP310HCbN
  • coal-ash
  • high-temperature corrosion