Abstract

Effects of mould temperature on microstructure and tensile properties of in situ thixoformed Sip/ZA27 composites were investigated. The results indicate that with the mould temperature increases, the solidification rate of ingot is decreased, and the size and fraction of the primary α-Al particles are increased. Moreover, Zn conent in the primary particles is increased. In addition, the aggregation tendency of Si particles tends to become serious. Based on tensile properties testing, the optimal mould temperature is 200℃, where the tensile strength and elongation reach up to 382 MPa and 1.17%, respectively. Moreover, the fracture mode of the thixoformed composites is transformed with the mould temperature increase.

Original languageEnglish
Pages (from-to)962-965 and 966
JournalTezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys
Volume35
Issue number9
DOIs
StatePublished - 20 Sep 2015
Externally publishedYes

Keywords

  • Microstructure
  • Mould temperature
  • Si/ZA27 composites
  • Tensile properties