Abstract
An investigation of the effect of the Si/B ratio on the microstructure and mechanical properties of high temperature Mo-Si-B alloys, doped with 0.9 wt.% lanthanum oxide (La2O3), is presented. Mechanical properties are measured at room temperature for three α-Mo-Mo 3Si-Mo5SiB2 containing alloys produced by powder metallurgy processing. It is found that the alloys with Si/B ratios of 2.4 and 1.4 possess a continuous α-Mo matrix with homogeneously distributed intermetallic particles while the alloy with the Si/B ratio of 0.7 is a homogeneous mix of α-Mo, Mo3Si and Mo5SiB 2 phases without continuous ones obsevered. Measurements on mechanical properties show that the flexural and compression strength, and fracture toughness of Mo-Si-B alloys were increased with the Si/B ratio raised. The continuous α-Mo phase with high volume fraction is beneficial for ameliorating the room temperature strength and fracture toughness.
| Original language | English |
|---|---|
| Pages (from-to) | 217-221 |
| Number of pages | 5 |
| Journal | Journal of Alloys and Compounds |
| Volume | 577 |
| DOIs | |
| State | Published - 2013 |
Keywords
- Lanthanum oxide
- Mechanical property
- Microstructure
- Mo-Si-B alloys
Fingerprint
Dive into the research topics of 'Effect of Si/B ratio on the microstructure and mechanical properties of lanthanum oxide-doped Mo-Si-B alloys'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver