Abstract
Micro-arc oxidation films are fabricated on the surface of AZ31B magnesium alloy in the Na 2 SiO 3 electrolyte. The mechanical performance of magnesium alloy bonding with the adhesive is examined by single lap-shear test, and the morphology and composition of the oxidation film are characterized by scanning electron microscope (SEM), energy dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD). The data indicate that the increase of Na 2 SiO 3 solution concentration results in the decrease of bonding strength of magnesium alloy joints, while the porosity has no directly relation with the variation of the lap-shear strength. The results also show that Na 2 SiO 3 participates into the film formation and the fabricated film is mainly composed of MgO and Mg 2 SiO 4 . In particular, with the increase of Na 2 SiO 3 solution concentration, the content of MgO decreased while that of Mg 2 SiO 4 increased. Moreover, MgO could initiate the formation of the hydroxyl group, which potentially enhances surface wettability and hydrogen bonding with the adhesive. This rationale is strongly supported by the results of Fourier Transform infrared spectra (FTIR), X-ray photoelectron spectroscopy (XPS) and contact angle measuring.
| Original language | English |
|---|---|
| Pages (from-to) | 447-452 |
| Number of pages | 6 |
| Journal | Applied Surface Science |
| Volume | 314 |
| DOIs | |
| State | Published - 30 Sep 2014 |
Keywords
- AZ31B magnesium alloy
- Bonding strength
- Micro-arc oxidation film
Fingerprint
Dive into the research topics of 'Effect of Na 2 SiO 3 solution concentration of micro-arc oxidation process on lap-shear strength of adhesive-bonded magnesium alloys'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver