In this work, ultrafine-grain WC-6Co/AlCoCrCuFeNi cemented carbides have been fabricated by spark plasma sintering method. The sintered samples are mainly composed of WC and the binder phase. With AlCoCrCuFeNi high-entropy alloy (HEA) increasing from 0 to 6 wt%, the binder phase transforms from Co to FCC solid solution phase rich in Co, Cu, Fe and Ni. Additionally, (Al, Cr)2O3 oxides and η phase form among the WC grains. Average equivalent diameter of WC grains decreases gradually from 358.2 to 271.7 nm. This is mainly because the solubility of W and C in HEA binder phase is much lower and their diffusion can be better hindered due to the sluggish effect. Thus, the dissolution-precipitation-growth process of WC can be effectively inhibited. On the other hand, the formation of (Al, Cr)2O3 oxides and η phase along WC grain boundaries can impede their abnormal growth. Consequently, the hardness can be improved while the fracture toughness decreases. WC grain refinement, higher hardness of HEA and formation of hard phases ((Al, Cr)2O3 oxides and η phase) account for the hardness improvement. The decreased fracture toughness is attributed to the weak interface bonding between WC and oxides, formation of brittle η phase and lower relative density. Furthermore, the transversal rupture strength (TRS) decreases with HEA addition while compressive strength (CS) can be improved. By comparison, WC-2Co4HEA sample shows relatively better comprehensive mechanical properties, with hardness, fracture toughness, TRS and CS of 2185.75 HV30, 10.47 MPa m1/2, 1717.12 MPa and 3054.25 MPa, respectively.

Original languageEnglish
Pages (from-to)4081-4095
Number of pages15
JournalJournal of Materials Research and Technology
Volume41
DOIs
StatePublished - 1 Mar 2026

Keywords

  • High-entropy alloys
  • Mechanical properties
  • Microstructure
  • Spark plasma sintering
  • Ultrafine-grain WC cemented carbides

Fingerprint

Dive into the research topics of 'Effect of HEA addition on the microstructure evolution and mechanical properties of SPSed ultrafine-grain WC-6Co cemented carbide'. Together they form a unique fingerprint.

Cite this