Abstract
Micron-sized internal cracks were introduced into pure magnesium specimens with equiaxial grains by uniaxial symmetric tension-compression plastic-strain-controlled fatigues at room temperature. These cracks are within the grains or across the grain. boundaries, and their widths are within the range of 0.5-1.5 μm, and the aspect ratios of length-to-width are within the range of 10-35. The as-fatigued specimens were then annealed in vacuum at 623 K from 2 to 6.5 h. SEM observations show that the two-dimensional longitudinal section of the intragranular microcracks evolves from the original thin-ellipse shape into the several aligned spherical voids dominated by surface diffusion. The transgranular microcracks break into two parts at the site of grain boundary dominated by surface diffusion coupled with grain boundary diffusion, and a single void was left on the grain boundary. During the late annealing, the shrinkage of the resultant voids brings an increase in the void-to-void spacing and further a somewhat recovery in the sample density.
| Original language | English |
|---|---|
| Pages (from-to) | 819-823 |
| Number of pages | 5 |
| Journal | Jinshu Xuebao/Acta Metallurgica Sinica |
| Volume | 41 |
| Issue number | 8 |
| State | Published - Aug 2005 |
Keywords
- Diffusive healing
- Internal fatigue micro crack
- Pure magnesium
Fingerprint
Dive into the research topics of 'Diffusive healing of internal fatigue microcracks in pure magnesium'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver