Breakdown Voltage Enhancement of Vertical Diamond Schottky Barrier Diode With Annealing Method and Al2O3 Field Plate Structure

  • Qi Li
  • , Juan Wang
  • , Guoqing Shao
  • , Genqiang Chen
  • , Shi He
  • , Qianwen Zhang
  • , Shumiao Zhang
  • , Ruozheng Wang
  • , Shuwei Fan
  • , Hong Xing Wang
  • Xi'an Jiaotong University

Research output: Contribution to journal › Article › peer-review

28 Scopus citations

Abstract

We proposed a simple method to enhance the breakdown voltage (BV) and reduce the turn-on voltage (VON) for diamond vertical Schottky barrier diode (SBD) with Al2O3 field plate (FP) structure. The Al2O3 was deposited by atomic layer deposition at 200 ◦C. Ti/Pt/Au and Zr/Ni/Au metal stacks were used as ohmic and Schottky electrodes, respectively. Then, this FP terminated SBD was annealed at 400 ◦C to improve Al2O3 quality and lower Schottky barrier height. The ideality factor and Schottky barrier height are 1.60 and 1.42 eV, respectively. Compared with regular diamond SBD, the BV of annealed diamond SBD was enhanced from 162 V to 386 V with an increasement of 138%, and the VON was decreased from −2.30 to −1.65 V. This method is potential for the development of diamond power devices.

Original languageEnglish
Pages (from-to)1937-1940
Number of pages4
JournalIEEE Electron Device Letters
Volume43
Issue number11
DOIs
StatePublished - 1 Nov 2022

Keywords

  • AlO
  • Diamond
  • annealing
  • breakdown voltage
  • schottky barrier diode

Fingerprint

Dive into the research topics of 'Breakdown Voltage Enhancement of Vertical Diamond Schottky Barrier Diode With Annealing Method and Al2O3 Field Plate Structure'. Together they form a unique fingerprint.

Cite this