Behavior mechanism and prediction models of stress corrosion cracking of stainless steels in pressurized water reactors

  • Pengfei Gao
  • , Yanhui Li
  • , Zhouyang Bai
  • , Shaoming Ding
  • , Yinan Zhang
  • , Limei Xing
  • , Zhihong Yu
  • Xi'an Jiaotong University
  • University of California at Berkeley

Research output: Contribution to journal › Review article › peer-review

6 Scopus citations

Abstract

Stress corrosion cracking (SCC) which has long been an essential topic for alloys exposed to subcritical water systems,is an urgent issue for pressurized water reactors (PWRs). Due to the complexity of the interaction of materials, environment, and stress, the SCC mechanism of consensus and the prediction model with mechanic extensibility are unavailable. Based on reviewing the typical characteristics and critical influence factors of SCC of stainless steels, this paper systematically summarizes, compares the more mainstream cracking mechanisms, and from the perspective of empirical and deterministic methods, discusses the applicable conditions of a series of SCC prediction models with high recognition via practical data, which are of great significance for strengthening readers’ understanding of SCC critical parameters and the matching service environment of each SCC mechanism, promoting the accurate prediction of SCC behavior and cumulative damage in the pressurized water reactors.

Original languageEnglish
Article number113897
JournalNuclear Engineering and Design
Volume434
DOIs
StatePublished - 1 Apr 2025

Keywords

  • Cracking mechanism
  • Cracking prediction
  • Hydrochemical environment
  • Pressurized water reactor
  • Stress corrosion cracking
  • Subcritical water systems