Abstract
The properties of metal hydride materials will be significantly degenerated by the poisoning effect of impurity gases such as CO, O2, H2S, etc. However, there are few reports on the poisoning kinetic model of metal hydride, which is important for the high-purity hydrogen purification and production from industry H2-contained waste gas. Hence, in this work, a novel poisoning hydrogen absorption kinetic model for metal hydride running in the CO + H2 mixture gas is developed, which considers the effect of poisoning on the volume growth rate of the product phase based on classical Johnson-Mehl-Avrami model. The novel model is also validated by comparison with experimental data of hydrogen absorption of LaNi4.3Al0.7 in a hydrogen atmosphere containing CO (∼0.1% v/v). The comparison results showed good agreement between model and experiment in the temperature range of 323–403 K. Based on experimental data and model, the reaction mechanism and rate-controlling steps of LaNi4.3Al0.7 hydrogenation process with 0.1%v/v CO were further uncovered.
| Original language | English |
|---|---|
| Article number | 132751 |
| Journal | Journal of Cleaner Production |
| Volume | 365 |
| DOIs | |
| State | Published - 10 Sep 2022 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Keywords
- Hydrogenation behavior
- Kinetic model
- Metal hydride
- Poisoning
Fingerprint
Dive into the research topics of 'Absorption of poisoned hydrogen from metal hydride under CO+H2 mixture gas for the production of clean, high purity hydrogen'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver